EN 10025-2 standard

W.NR.: 10070

Non-alloy steel for structural purposes

heat analysis according to the EN 10025-2 standard

  C % Si % Mn % P % S % N % Cu %
From
To 0,045 0,045 0,012

according to the UNI 10233-3 standard

Thickness mm Cold drawn
( +C )
Rp0,2  minimum Rm minimum A5 %
(MPa) (MPa)
≤5 745 880 ÷ 1.180 5
>5≤10 670 835 ÷ 1.130 5
>10≤16 560 785 ÷ 1.080 6
>16≤25 520 785 ÷ 1.030 6
>25≤40 450 735 ÷ 980 7
>40≤80 370 715 ÷ 960 8
>80

* Delivery condition: as rolled.

Weldability:
Failing any prescriptions concerning chemical composition, no technical data about this steel weldability are available.

Notes:

CORRESPONDENCE WITH OTHER STANDARDS (purely as an indication):

EN 10025-2:04 EN 10025:90 UNI 7070 DIN 17 100 NF A35-501
 E360  Fe 690-2  Fe 690  St 70-2  A 70-2

E360.pdf