EN 10277-2 standard

W.NR.: 1.0122

Non-alloy steel for structural purposes

heat analysis according to the EN 10277-2 standard

  C % Si % Mn % P % S % N % Cu %
per spessori in mm
 ≤40              >40
From
To 0,17 0,20 1,40 0,040 0,040 0,012 0,55

according to the EN 10277-2 standard

Thickness mm Rolled + peeled rolled
( +SH )
Cold drawn
( +C )
hardness HB Rm (MPa) Rp0,2  minimum Rm (MPa) A5 %
(MPa) minimum
≥5≤10 355 da 470 a 840 8
>10≤16 300 da 420 a 770 9
>16≤40 da 102 a 140 da 360 a 510 260 da 390 a 730 10
>40≤63 da 102 a 140 da 360 a 510 235 da 380 a 670 11
>63≤100 da 102 a 140 da 360 a 510 215 da 360 a 640 11

* Delivery condition: as rolled.

Weldability:
This steel grade is generally suitable to welding.

Notes:

CORRESPONDENCE WITH OTHER STANDARDS (purely as an indication):

 

EN 10025-2:04
 S235JR

S235JRC.pdf